This steel ball must hit the field area of the shingle two times and the edge of the shingles two times without damaging the mat to qualify for a particular class rating.
Level 3 4 roofing.
Class 4 roof covering is the most impact resistant roof and receives the highest premium discount.
Roofing screw 28 special interest promotional items 35 roofing screws.
Architectural shingles are a step up from 3 tab shingles.
Roof coverings that have passed the ul standard 2218 test are classified as either class 1 2 3 or 4.
Low profile head reduces damage to installation and single ply membrane when attaching to steel or timber.
Class 1 would be the lowest tested rating.
A fiberglass mat has proven to be a more sustainable effective product.
Durecorder live scienceandsuperhero pvz game durecorder live please like dislike subscribe comment share this video instagram.
A class 4 roof covering receives the highest premium credit.
Ul class 1 2 3 and 4 tx only ul and fm class 3 and 4 all other states.
A class 4 rating the material should not get damaged when hit twice in the same spot by 2 inch diameter steel ball.
Standard entry level 3 tab shingles are the cheapest and thinnest.
4 3 8 black epoxy 51605 pkg.
Class 4 roofing shingles are considered to be a premium product and therefore may cost more than standard non impact resistant shingles.
Roof coverings that have passed the ul standard 2218 test are classified by ul as either class 1 2 3 or 4.
Level 3 nvq diploma in roofing occupations roof slater and tiler level 3 nvq diploma in roofing occupations thatching use the form at the top of the page and get a quote on the price of the roofing nvq.
Summarizing the result we would be looking at for a class 3 roof is earned if the sample does not crack when hit twice in the same spot by a 1 75 inch diameter steel ball.
The list of approved laboratories is shown below.
They re slightly thicker and made to resemble more expensive wood shakes.
Approved laboratory roof class location.